Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 758 cP @Temperature 35.0 °C |
758 cP @Temperature 95.0 °F |
|
BASF Pluracol® 1168 Rigid Polyol Description: Pluracol® 1168 Polyol is a general purpose aromatic initiator-based polyol for rigid foams for use in a variety of applications. It is attractively priced for consideration for foaming.. |