Polymer Property : Viscosity = 742560 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 742560 cP

@Shear Rate 500 1/s,
Temperature 250 °C
742560 cP

@Shear Rate 500 1/s,
Temperature 482 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide..