Physical Properties Metric English Comments
Viscosity 74000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
74000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Viscosity 74000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
74000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynaflex™ G7690-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7690-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Viscosity 74000 cP

@Shear Rate 10000 1/s,
Temperature 260 °C
74000 cP

@Shear Rate 10000 1/s,
Temperature 500 °F
ISO 11443
DuPont Performance Polymers Crastin® SK609 NC010 PBT  (Unverified Data**)
Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Viscosity 74000 cP

@Shear Rate 5000 1/s,
Temperature 270 °C
74000 cP

@Shear Rate 5000 1/s,
Temperature 518 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved