Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 7250 cP @Temperature 25.0 °C |
7250 cP @Temperature 77.0 °F |
|
Dow VORALUX™ HL 430 Copolymer Polyol VORALUX™ HL 430 is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile and filtered to 100 microns. It is used in the manufacture of flexible slabstock polyurethan.. |