Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 6700 cP @Shear Rate 11200 1/s, Temperature 200 °C |
6700 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |