Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 664000 cP @Shear Rate 700 1/s, Temperature 275 °C |
664000 cP @Shear Rate 700 1/s, Temperature 527 °F |
DAM; ISO 11443 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |