Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 600000 cP @Shear Rate 1000 1/s, Temperature 280 °C |
600000 cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
DSM Akulon® F230-C PA6 Medium Viscosity, Extrusion, Injection Molding |
|||
Viscosity | 600000 cP @Shear Rate 1.00 1/s, Temperature 270 °C |
600000 cP @Shear Rate 1.00 1/s, Temperature 518 °F |
|
DSM Arnite® TV4 461 (PBT+PET)-GF30 30% Glass Reinforced |
|||
Viscosity | 600000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
600000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Novamid® 2420A PA666 Extrusion |
|||
Viscosity | 600000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
600000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Novamid® 2420J PA666 Extrusion |