Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 6000 cP @Temperature -30.0 °C |
6000 cP @Temperature -22.0 °F |
CCS |
ExxonMobil Mobil Clean 5W-30 High Mileage Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and.. |
|||
Viscosity | 6000 cP @Temperature -20.0 °C |
6000 cP @Temperature -4.00 °F |
CCS; ASTM D5293 |
ExxonMobil Mobil Delvac 15W-40 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |
|||
Viscosity | 6000 cP @Temperature -30.0 °C |
6000 cP @Temperature -22.0 °F |
CCS |
ExxonMobil Mobil Clean 5W-30 High Mileage Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and.. |
|||
Viscosity | 6000 cP @Temperature -20.0 °C |
6000 cP @Temperature -4.00 °F |
CCS; ASTM D5293 |
ExxonMobil Mobil Delvac 15W-40 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |
|||
Viscosity | 6000 cP @Temperature 25.0 °C |
6000 cP @Temperature 77.0 °F |
at 20 rpm vibration |
Permabond A131 Anaerobic Threadsealant Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an.. |