Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5760 cP @Temperature -25.0 °C |
5760 cP @Temperature -13.0 °F |
CCS |
ExxonMobil Mobil Clean 10W-30 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Viscosity | 5760 cP @Temperature -25.0 °C |
5760 cP @Temperature -13.0 °F |
CCS |