Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 56080 cP @Shear Rate 5000 1/s, Temperature 230 °C |
56080 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |