Polymer Property : Viscosity = 560000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 560000 cP

@Shear Rate 316 1/s,
Temperature 275 °C
560000 cP

@Shear Rate 316 1/s,
Temperature 527 °F
ISO 11443
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..