Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 55190 cP @Shear Rate 5000 1/s, Temperature 260 °C |
55190 cP @Shear Rate 5000 1/s, Temperature 500 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |