Polymer Property : Viscosity = 525 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 525 cP

@Temperature 37.8 °C
525 cP

@Temperature 100 °F
BASF Pluracol® 628 Specialty Polyol
Description: Pluracol® 628 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 628 can also be used ..