Physical Properties Metric English Comments
Viscosity 51430 cP

@Shear Rate 5000 1/s,
Temperature 290 °C
51430 cP

@Shear Rate 5000 1/s,
Temperature 554 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers