Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 501000 cP @Shear Rate 700 1/s, Temperature 295 °C |
501000 cP @Shear Rate 700 1/s, Temperature 563 °F |
DAM; ISO 11443 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |