Physical Properties Metric English Comments
Viscosity 30 - 50 cP

@Temperature 20.0 °C
30 - 50 cP

@Temperature 68.0 °F
Uncured
Permabond 931 Cyanoacrylate
PERMABOND 931 is a low odor, non­fogging, non­frosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv..
Viscosity 15 - 50 cP

@Time 119 sec
15 - 50 cP

@Time 0.0330 hour
V-128-1
Solvay JAGUAR® 418 Surfactant
Description: Nonyl Jaguar 418 is a carboxymethylhydroxypropyl guar with extremely low residue and dual cross-linking capability. When dispersed into water with agitation it will wet out and hydrate ..
Viscosity 22 - 50 cP

@Time 241 sec
22 - 50 cP

@Time 0.0670 hour
V-128-1
Solvay JAGUAR® 418 Surfactant
Description: Nonyl Jaguar 418 is a carboxymethylhydroxypropyl guar with extremely low residue and dual cross-linking capability. When dispersed into water with agitation it will wet out and hydrate ..
Viscosity 31 - 50 cP

@Time 3600 sec
31 - 50 cP

@Time 1.00 hour
V-128-1
Solvay JAGUAR® 418 Surfactant
Description: Nonyl Jaguar 418 is a carboxymethylhydroxypropyl guar with extremely low residue and dual cross-linking capability. When dispersed into water with agitation it will wet out and hydrate ..
Viscosity 31 - 50 cP

@Time 86400 sec
31 - 50 cP

@Time 24.0 hour