Polymer Property : Viscosity = 5.00e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Novamid® 2430A PA666
Film Extrusion, Extrusion, Extrusion Grade
Viscosity 5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Novamid® 2430A-1 PA666
Film Extrusion, Extrusion, Extrusion Grade
Viscosity 5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Novamid® 2430AH2 PA666
Film Extrusion, Extrusion, Extrusion Grade
Viscosity 5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Novamid® 2430J PA666
Film Extrusion, Extrusion, Extrusion Grade
Viscosity 5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
5.00e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Novamid® 2430A PA666
Film Extrusion, Extrusion, Extrusion Grade