Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.0 - 5.0 cP @Temperature 20.0 °C |
1.0 - 5.0 cP @Temperature 68.0 °F |
Uncured |
Permabond 930 Cyanoacrylate PERMABOND 930 is a low odor, nonfogging, nonfrosting cyanoacrylate. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The .. |