Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 480900 cP @Shear Rate 500 1/s, Temperature 225 °C |
480900 cP @Shear Rate 500 1/s, Temperature 437 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |