Physical Properties Metric English Comments
Viscosity 44000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
44000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Viscosity 44000 cP

@Shear Rate 5000 1/s,
Temperature 300 °C
44000 cP

@Shear Rate 5000 1/s,
Temperature 572 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough..
Viscosity 44000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
44000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2503.10 Polyethylene resin is a narrow molecular weight distribution copolymer designed as a superior processing resin. For very thin wall higher cavitation molding, this grade often is a p..
Viscosity 44000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
44000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow LDPE 955I Low Density Polyethylene
DOW LDPE 955I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility, and good toughness, with low warpage. Typical applications include lid..
Viscosity 44000 cP

@Shear Rate 5000 1/s,
Temperature 320 °C
44000 cP

@Shear Rate 5000 1/s,
Temperature 608 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 330 NC010 Nylon  (Unverified Data**)
Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers