Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 43970 cP @Shear Rate 5000 1/s, Temperature 300 °C |
43970 cP @Shear Rate 5000 1/s, Temperature 572 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |