Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 42800 cP @Shear Rate 1340 1/s, Temperature 200 °C |
42800 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G2701C Thermoplastic Elastomer (TPE) Dynaflex™ G2701C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Rubbery Feel.. |
|||
Viscosity | 42800 cP @Shear Rate 1340 1/s, Temperature 200 °C |
42800 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |