Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 407000 cP @Shear Rate 500 1/s, Temperature 215 °C |
407000 cP @Shear Rate 500 1/s, Temperature 419 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler with high stiffness low warpage and low creep for sup.. |