Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 406500 cP

@Shear Rate 500 1/s,
Temperature 250 °C
406500 cP

@Shear Rate 500 1/s,
Temperature 482 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate  Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b..
Viscosity 406500 cP

@Shear Rate 500 1/s,
Temperature 250 °C
406500 cP

@Shear Rate 500 1/s,
Temperature 482 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate  Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b..