Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4.2 cP @Temperature 82.2 °C |
4.2 cP @Temperature 180 °F |
|
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |