Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4.14e+6 cP @Shear Rate 0.100 1/s, Temperature 190 °C |
4.14e+6 cP @Shear Rate 0.100 1/s, Temperature 374 °F |
0.1 rad/sec; ARES Rheometer |
Dow Engage® ENX 7458.00 Ethylene-Butene Copolymer Description: ENX 7458.00 is a unique broader molecular weight distribution ethylene-butene copolymer that offers excellent flow and impact properties and is ideally suited for plastics modification... |