Viscosity 360000 - 380000 cP

@Temperature 260 - 260 °C
360000 - 380000 cP

@Temperature 500 - 500 °F
Average value: 370000 cP Grade Count:2
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Viscosity 360000 - 380000 cP

@Shear Rate 1000 - 1000 1/s
360000 - 380000 cP

@Shear Rate 1000 - 1000 1/s
Average value: 370000 cP Grade Count:2
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..