Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 355 cP @Temperature 35.0 °C |
355 cP @Temperature 95.0 °F |
|
BASF Pluracol® 4156 Slabstock Foam Polyol Description: Pluracol® 4156 polyol is a 56 hydroxyl number (nominal 3000 molecular weight) polyether triol capable of producing a broad range of flexible slabstock polyurethane foams for furniture,.. |