Physical Properties Metric English Comments
Viscosity 70541.6 - 351621 cP

@Temperature 250 - 270 °C
70541.6 - 351621 cP

@Temperature 482 - 518 °F
Average value: 195000 cP Grade Count:1
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..
Viscosity 70541.6 - 351621 cP

@Shear Rate 500 - 5000 1/s
70541.6 - 351621 cP

@Shear Rate 500 - 5000 1/s
Average value: 195000 cP Grade Count:1
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..