Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 300000 - 350000 cP @Temperature 280 - 280 °C |
300000 - 350000 cP @Temperature 536 - 536 °F |
Average value: 325000 cP Grade Count:2 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Viscosity | 300000 - 350000 cP @Shear Rate 1000 - 1000 1/s |
300000 - 350000 cP @Shear Rate 1000 - 1000 1/s |
Average value: 325000 cP Grade Count:2 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |