Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 340700 cP @Shear Rate 500 1/s, Temperature 250 °C |
340700 cP @Shear Rate 500 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |