Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3400 cP @Temperature 82.2 °C |
3400 cP @Temperature 180 °F |
|
Northstar Polymers MPA-135 MDI Ether Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 3400 cP @Temperature 25.0 °C |
3400 cP @Temperature 77.0 °F |
|
BASF Pluracol® 1158 Specialty Polyol Description: Pluracol® 1158 polyol is a polyol which can be used in a wide variety of applications. It can be employed as a cross-linking agent for rigid foam as well as coatings and elastomers. Wh.. |