Polymer Property : Viscosity = 330000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 200 - 330000 cP

@Temperature 275 - 280 °C
200 - 330000 cP

@Temperature 527 - 536 °F
Average value: 83300 cP Grade Count:2
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Viscosity 200 - 330000 cP

@Shear Rate 10.0 - 1000 1/s
200 - 330000 cP

@Shear Rate 10.0 - 1000 1/s
Average value: 83300 cP Grade Count:2
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..