Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3300 cP @Temperature 220 °C |
3300 cP @Temperature 428 °F |
|
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive Self-extinguishing version of 3748 and Meets UL 1410 requirementsInformation provided by 3M |