Polymer Property : Viscosity = 33 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 33 cP

@Temperature 180 °C
33 cP

@Temperature 356 °F
Melt (Unpolymerized resin); Cone and plate 10 1/s shear rate
Cyclics CBT® 100 Thermoplastic Resin
CBT® 100 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between..