Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 321800 cP @Shear Rate 500 1/s, Temperature 240 °C |
321800 cP @Shear Rate 500 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |