Polymer Property : Viscosity = 320 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 320 cP

@Shear Rate 10.0 1/s,
Temperature 300 °C
320 cP

@Shear Rate 10.0 1/s,
Temperature 572 °F
shear rate: 10/s
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Viscosity 320 cP

@Temperature 40.0 °C
320 cP

@Temperature 104 °F
Teknor Apex TruVis Esters™ TTDTM Tri-Tridecyl Trimellitate