Physical Properties Metric English Comments
Viscosity 30700 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
30700 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE)
Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p..