Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 21000 - 305000 cP @Temperature 190 - 190 °C |
21000 - 305000 cP @Temperature 374 - 374 °F |
Average value: 91600 cP Grade Count:8 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Viscosity | 21000 - 305000 cP @Shear Rate 300 - 5000 1/s |
21000 - 305000 cP @Shear Rate 300 - 5000 1/s |
Average value: 91600 cP Grade Count:8 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |