Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 301100 cP @Shear Rate 500 1/s, Temperature 240 °C |
301100 cP @Shear Rate 500 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |