Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 20 - 30 cP @Temperature 120 °C |
20 - 30 cP @Temperature 248 °F |
|
Abatron AboCast/AboCure 8109-5 High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications.. |