Polymer Property : Viscosity = 3.31 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 3.31 cP

@Temperature 110 °C
3.31 cP

@Temperature 230 °F
Solvay Chemicals Glycerol alpha monochlorohydrin
Viscous liquid used as chemical intermediate.EINECS Number: 202-492-4/CAS Number: 96-24-2/UN number: 2689Information provided by Solvay