Polymer Property : Viscosity = 299000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 299000 cP

@Shear Rate 1000 1/s,
Temperature 275 °C
299000 cP

@Shear Rate 1000 1/s,
Temperature 527 °F
DAM; ISO 11443
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers