Physical Properties Metric English Comments
Viscosity 290000 cP

@Temperature 25.0 °C
290000 cP

@Temperature 77.0 °F
ET538A, Epoxy Resin
Permabond ET538 Epoxy Resin
PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia..
Viscosity 290000 cP

@Shear Rate 500 1/s,
Temperature 275 °C
290000 cP

@Shear Rate 500 1/s,
Temperature 527 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers