Polymer Property : Viscosity = 284000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 284000 cP

@Shear Rate 500 1/s,
Temperature 275 °C
284000 cP

@Shear Rate 500 1/s,
Temperature 527 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..