Polymer Property : Viscosity = 238600 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 238600 cP

@Shear Rate 500 1/s,
Temperature 270 °C
238600 cP

@Shear Rate 500 1/s,
Temperature 518 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers