Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 225 cP

@Temperature 54.5 °C
225 cP

@Temperature 130 °F
BASF Pluracol® 816 Molded Foam Polyol
Description: Pluracol® 816 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol ..
Viscosity 225 cP

@Temperature 54.4 °C
225 cP

@Temperature 130 °F
BASF Pluracol® 1421 Molded Foam Polyol
Description: Pluracol® 1421 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol..