Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 17000 - 22000 cP @Shear Rate 1.00 1/s, Temperature 25.0 °C |
17000 - 22000 cP @Shear Rate 1.00 1/s, Temperature 77.0 °F |
LVF#4, Uncured |
Fibre Glast 180 Clear Gel Coat #180 Clear Gel Coat is a high performance, premium quality gel coat for both airless and air atomized spray applications. #180 offers UV light stability, excellent clarity, crack and chemical resist.. |