Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2200 - 3000 cP @Shear Rate 30.0 1/s, Temperature 40.0 °C |
2200 - 3000 cP @Shear Rate 30.0 1/s, Temperature 104 °F |
P-3500 LCD MB3; 25 wt% polymer solution in DMAc |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
Viscosity | 2200 cP @Shear Rate 10.0 1/s, Temperature 270 °C |
2200 cP @Shear Rate 10.0 1/s, Temperature 518 °F |
|
Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |