Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 219300 cP @Shear Rate 500 1/s, Temperature 270 °C |
219300 cP @Shear Rate 500 1/s, Temperature 518 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |